Author Topic: I made a nice set of beads.......and then...  (Read 658 times)
0 Members and 1 Guest are viewing this topic.
Princess Peggy
Dancing With Glass
Forum Member
*******
Posts: 1231


Totally devoted to glass.


WWW
« on: October 11, 2011, 01:37:31 PM »

.....found one of them had cracked!   I'm so cross!  I just find it so hard to keep them from cracking while I'm decorating them.  Mind you, I can blame the dog doing a poo on the carpet when I was half way through.  I put it back in the kiln while I was dealing with it!


PA110240 by Princess Peggy1, on Flickr

( At first I thought it was two of them but I was so put out I think I picked the same one up twice.!)
« Last Edit: October 11, 2011, 01:44:52 PM by Princess Peggy » Logged

Jennie Lamb
Raspberry Rings
Forum Member
******
Posts: 813



WWW
« Reply #1 on: October 11, 2011, 01:44:48 PM »

LOL!! Bad luck but that made me laugh so much naughty doggie!!  Their timing is never right is it!!
Logged


Feather bead Tutorial now Available www.raspberryrings.etsy.com, www.facebook.com/raspberryrings
chipperpottery
Life passes by when melting glass.
Forum Member
********
Posts: 2036


WWW
« Reply #2 on: October 11, 2011, 01:45:22 PM »

O'h I would have been so upset, they are super.
Logged

Princess Peggy
Dancing With Glass
Forum Member
*******
Posts: 1231


Totally devoted to glass.


WWW
« Reply #3 on: October 11, 2011, 01:45:49 PM »

To be fair she had put her head round the door to let me know but I ignored her.
Logged

tomcat
While the rest of the species is decended from apes redheads are decended from cats
Forum Member
*****
Posts: 550


The tom of three cats


WWW
« Reply #4 on: October 11, 2011, 01:52:13 PM »

I can blame the dog doing a poo on the carpet when I was half way through.  I put it back in the kiln while I was dealing with it!

just to take this out of context - what did you put back in the kiln Grin
Logged

Mark - 3catsjewellery.com
Life is not a game - its THE game, so play it like you mean it
Princess Peggy
Dancing With Glass
Forum Member
*******
Posts: 1231


Totally devoted to glass.


WWW
« Reply #5 on: October 11, 2011, 03:33:30 PM »

Well the poo of course!!  What else could I have done with it?
Logged

Margram
Temperature's rising
Forum Member
********
Posts: 2671


Glass in pocket


« Reply #6 on: October 11, 2011, 04:33:48 PM »

 Grin Nice beads - shame about the cra.......ck Wink
Logged

Princess Peggy
Dancing With Glass
Forum Member
*******
Posts: 1231


Totally devoted to glass.


WWW
« Reply #7 on: October 11, 2011, 08:14:14 PM »

 Grin Grin Grin
Logged

Passionatelamper
Passionate lamper
Forum Member
*******
Posts: 1149


Carp Diem!


WWW
« Reply #8 on: October 11, 2011, 08:53:25 PM »

Giggling here....sorry about your bead though Peggy as the ones you did are cracking!!!!! Sorry!  Undecided Grin Cheesy
Logged

The Tartan Trout
Forum Member
******
Posts: 997



« Reply #9 on: October 11, 2011, 08:55:20 PM »

lovely beads, poor desperate doggie Sad
Logged

Kathy
Forum Member
****
Posts: 312



« Reply #10 on: October 11, 2011, 09:04:39 PM »

Ooh, such pretty colours - bloomin's kids and dogs! Wink
Logged
Pat from Canvey
Only a little bit odd
Forum Member
********
Posts: 2461


Keep on blowing


« Reply #11 on: October 12, 2011, 07:57:46 AM »

That's why I like cats. They poo in their litter tray, I pick it up in a poop scoop and put it down the toilet. I've always wondered why dogs don't have litter trays.
Logged

Studio Girl
Forum Member
****
Posts: 360



WWW
« Reply #12 on: October 12, 2011, 08:13:30 AM »

Really nice beads love the colours
Logged

jammie
Do what you can, with what you have, where you are
Forum Member
********
Posts: 3022



WWW
« Reply #13 on: October 12, 2011, 08:16:05 AM »

they're really nice too!  Smiley
Logged

Mand
Mandmade - that's me.
Forum Member
*******
Posts: 1008


Go f'rit!


WWW
« Reply #14 on: October 12, 2011, 01:45:02 PM »

They're beautiful ... shame about the cracked one though!