Pat, believe me, my bases are anything but good!  :D From the experience I have had, I'd say you need a very symmetrical bubble, then to pop a very even lip to spin out (any non-symmetrical-ness throws the spin off), and then to spin evenly and with an even heat gradient. It's tricky and frustrating, as my glass bin would show you!