Author Topic: Kiln Overshooting  (Read 2072 times)
0 Members and 1 Guest are viewing this topic.
*Nicky*
Guest
« on: March 22, 2007, 02:29:27 PM »

Hiya,

Second time its done it now, but my kiln keeps over shooting the set 510 temp when on a full ramp - any ideas ?

Ta
Logged
beadysam
BeadySamGlass.Com
Forum Member
******
Posts: 754


I type before I think....


WWW
« Reply #1 on: March 22, 2007, 02:45:34 PM »

Is it overshooting by much?
Logged

beads-on-toast
Forum Member
****
Posts: 388


Dichroic Diva


WWW
« Reply #2 on: March 22, 2007, 03:39:05 PM »

mine varies around abour 50 degrees

goes down too 475 sometimes then back up to 525. or is it loads?
Logged

Caroline
Guest
« Reply #3 on: March 22, 2007, 04:09:49 PM »

mine varies around abour 50 degrees

goes down too 475 sometimes then back up to 525. or is it loads?

mine goes up and down a bit but not as much as yours Anna, mines never by more than 10
Logged
*Nicky*
Guest
« Reply #4 on: March 22, 2007, 04:15:20 PM »

Yeah, on the first full rame to 520 its going upto about 560 maybe a bit more, but the alarm kicks in and lets me know. After ive pressed the start button it comes back down again, then when i override the hold part to make it go up to 520 for annealling it does it again, maybe not as much about 10-20 more.

I suppose i just expected it to stay at the given temp, give or take a few as it trys to regulate itself.
Logged
Failariel
Forum Member
*******
Posts: 1231



WWW
« Reply #5 on: March 22, 2007, 04:46:38 PM »

Mine varies but I've never really taken much notice of by how much. I assumed it was the way the regulator was set up at the factory.
Logged

astringofbeads
Guest
« Reply #6 on: March 22, 2007, 04:48:37 PM »

Mine did that too Nicky went as high as 560 then the HDTE message came up, and in the end I had to adjust the first ramp to heat it up a bit more slowly. Since I did it it hasn't done it since. I figured mine didn't like getting that hot that quickly Grin
Mind you it's having wobblies of a different kind now, flippin thing!
Logged
beadysam
BeadySamGlass.Com
Forum Member
******
Posts: 754


I type before I think....


WWW
« Reply #7 on: March 22, 2007, 04:55:21 PM »

mine varies by about 10 degrees too...
Logged

Vicki
Forum Member
****
Posts: 412



WWW
« Reply #8 on: March 22, 2007, 07:42:23 PM »

Mine goes up & down too...must be the norm I guess Cheesy
Logged

Mary
Forum Member
******
Posts: 835



WWW
« Reply #9 on: March 22, 2007, 10:02:46 PM »

Maybe because it's new, Nicky? Mine used to get up to temp really fast, it takes a little longer now. Maybe try programming a slightly slower ramp?
Oh, and opening and closing the bead door makes it fluctuate, I just open my bead door and leave it till I'm finished, then close it as far as poss.
« Last Edit: March 22, 2007, 10:04:49 PM by Mary » Logged

Mary
beads-on-toast
Forum Member
****
Posts: 388


Dichroic Diva


WWW
« Reply #10 on: March 22, 2007, 10:29:47 PM »

yeah mine fluctuates cause of the bead door and because it is right next to the window.
bloomin freezing at the mo
Logged

ebj
Forum Member
***
Posts: 175



WWW
« Reply #11 on: March 22, 2007, 10:47:23 PM »

Mine overshot at first too - its stopped now though!

Emma
Logged

Emma

Art Clay Senior Instructor & Lampworker

www.emmabaird.wordpress.com
*Nicky*
Guest
« Reply #12 on: March 22, 2007, 11:08:40 PM »

Oh sounds normal then, thanks for that !
Logged
Bumpy Beads
Forum Member
***
Posts: 233



WWW
« Reply #13 on: March 23, 2007, 06:24:48 PM »

Mine is overshooting too. Is it contagious?? I used my kiln for the first time today. I got the HtdE message, so I added a segment to the beginning of the schedule that someone (Helen P?) kindly posted somewhere in this forum.

I added this:

Ramp1 700C
Temp1 410 C
Hold1 0.10

then;

Ramp2 FULL
Temp2 510 C
Hold2 6.00
Ramp3 FULL
Temp3 520C
Hold3 60mins
Ramp4 78 C
Temp4 371 C
Hold5 00mins
Ramp5 0000

Still with me? After running this schedule I got the HdtE message again. Any suggestions anyone? Undecided
 I'm making it up as I go along  Cheesy 
Logged

Dickie
I'm pink therefore I must be dressed in Lycra
Administrator
*******
Posts: 707


Pink Lycra Anyone?


WWW
« Reply #14 on: March 23, 2007, 10:40:03 PM »

I work for a controls company and know quite a lot about control theory...

My assumption is that the controllers on most kilns are not "tuned" to the kiln (i.e they are probably just using the standard control settings)
Having tuned a kiln controller (for Sarah (silverlemon)) I can tell you that they are very difficult to control, basically I am not surprised that they overshoot when ramping up, one way to avoid it is to make the first stage a ramp up at a "relatively" slow rate (say 20-40deg/min or less) this will ensure that the controller doesn't just blast the kiln with full on heat for 10-15 mins while it heats up.
If you do a ramp up to start, it is very unlikely that the kiln will overshoot.

Hope this helps, if you have any questions then please ask
Logged

Dickie-Oh yes! Follow me on Twitter @DickieDooda
Pages: [1] 2
  Print  
 
Jump to:  

Powered by MySQL Powered by PHP Powered by SMF 1.1.18 | SMF © 2013, Simple Machines Valid XHTML 1.0! Valid CSS!
Page created in 0.062 seconds with 20 queries.