Mand
Mandmade - that's me.
Forum Member
*******
Posts: 1008


Go f'rit!


WWW
« on: September 27, 2009, 05:13:55 PM »

Hi all,

Was just scouring the site for some piccies of cool colour effetre beads - I know some of you have had a play with the exciting new glass.  I was wondering what it looks like as a bead. Please do show.  Smiley Mand x
Logged

Failariel
Forum Member
*******
Posts: 1233



WWW
« Reply #1 on: September 30, 2009, 09:41:35 PM »

Lovely (naked) laguna

Mimosa clothed in Sam's frit

Disappointing strawberry shake, also clothed in Sam's frit

Interesting how the smaller beads don't display the characteristics of the hollow!




Logged

Failariel
Forum Member
*******
Posts: 1233



WWW
« Reply #2 on: September 30, 2009, 09:56:02 PM »

this is cobalt & laguna
you can see the striations in the laguna near the bottom and top (the middle is just peeking through the cobalt to the laguna underneath)

Logged

Kaz
Flame Off Show Off
Global Moderator
*******
Posts: 2773


Worth my weight in glass....


WWW
« Reply #3 on: October 01, 2009, 08:36:27 PM »

The top of this and the donuts are laguna - I got streaks which are nice

These are green tea

Kazx
Logged


www.cheekycherubdesigns.co.uk - www.cheekycherubdesigns.etsy.com - For murrini and de-stash - www.kazkebab.etsy.com

She's made of real glass. She got real real emotion. But my heart laughs I have that same sweet devotion!
Veebee
Superglassyfrittylisticgirlmakes beadsatrocious!
Forum Member
*******
Posts: 1047


Serial HotHead on bulk user and glass murderess.


WWW
« Reply #4 on: October 02, 2009, 09:03:20 PM »

This is dark fossil, I can't wait to play around with this one some more!

Logged

Web: http://www.veebeads.net
The UK home of Val Cox frit!!
Fritt Flickr group: http://www.flickr.com/groups/1647822@N25/
Lush!
Julie
Forum Member
********
Posts: 2559


Queen of Buttons :0)


WWW
« Reply #5 on: October 14, 2009, 03:04:39 PM »

Love the fossil and I've got the laguna too, was really surprised when it came out transparent and streaky!  Its nice, reminds me of Reichenbach Ocean.

I've got the Cherry and that turns disappointingly white too  Angry

I think the Green Tea is my favourite so far, there's no other palest softest green like it.

 